Yosun (Tianjin) Piping Engineering Co., Ltd. is one of the most credible manufacturers and suppliers of pressure vessel components in China. Please feel free to wholesale customized pressure vessel components at competitive price from our factory. If you have any enquiry about quotation, please feel free to email us.

 

Chemical Requirements

 
Composition, %
Grades 1 and 2
Grade 3
Grade 4
Carbon, max
0.30 0.35 0.30
Manganese
0.40-1.05 0.80-1.35 0.80-1.35
Phosphorus, max
0.025 0.025 0.025
Sulfur, max
0.025 0.025 0.025
Silicon
0.15-0.35 0.15-0.35 0.15-0.35

Mechanical Properties

1. General Requirements-Except when otherwise specified in accordance with Supplementary Requirement S2, the material shall conform to the requirements for mechanical properties prescribed in Table 2 when tested in accordance with the latest issue of Test Methods and Definitions A370 or Test Methods A1058 when the M suffix standard has been specified. The largest obtainable tension test specimen as specified in Test Methods and Definitions A370 or Test Methods A1058, as applicable, shall be used.

2.Specific Requirements-The number and location of tests are based on forging length, weight, and heat treatment, and shall be as prescribed below. The length and weight to be used for this purpose shall be the shipped length and weight of forgings produced individually or the aggregate shipped length and weight of all pieces cut from a multiple forging.

Heat Treatment

1.After forging and before reheating for heat treatment, the forgings shall be cooled in such a manner as to prevent injury and to accomplish transformation.

2.All forgings shall be annealed, normalized, or normalized and tempered, but alternatively may be liquid quenched and tempered when mutually agreed upon between the manufacturer and the purchaser. When tempering is performed, it shall be at a subcritical temperature, but no less than 1100°F [595°C].

3.A multiple stage austenitizing procedure may be used whereby the forging is first fully austenitized and liquid quenched, followed by reheating within the intercritical temperature range to partially reaustenitize, and again liquid quenched. On completion of the austenitizing/quenching cycles, tempering at a temperature between 1100°F [595°C] and the lower critical temperature shall follow.

Tensile Requirements

 
Grade 1
Grades
2 and 4
Grade 3
Tensile strength, min, ksi
[MPa]
60–85
[415–585]
70–95
[485–655]
75–100
[515–690]
Yield strength (0.2 % offset),
min, ksi [MPa]
30
[205]
36
[250]
37.5
[260]
Elongation in 2 in. [62.5
mm], min, %
23
[21]
20
[18] 
19
[17]
Reduction of area, min, %
38
33
30

 

 

Hot Tags: pressure vessel components, China pressure vessel components manufacturers, suppliers, harga elbow stainless 304 2 inch, 4 stainless exhaust elbow, 2 stainless elbow, 2 inch steel elbow, 10mm to 15mm copper elbow, compression reducing elbow 15mm to 10mm